ran into a problem??????

Posted by admin on October 2nd, 2009 at 11:08pm

I machined an item from 6061 . basically it is a ring (doughnut) with 6 bolt holes in the face, then counter sunk so the bolt head lays flush with the face.

I shot gloss black on them last night and had poor results. Around the machined edge of the countersink, the powder appeared to flow away…so…in essence, there is a hairline silver ring around each counter sink.

here is how I prepped:

1) scorch brited part
2) used brake cleaner
3) heated part to dry off any residue
4) powdered…cured

question: should I media blast the entire part to ensure the crisp edge of the counter sink gets etched?

Thanks

Related posts:

  1. Zinc Plating Problems I am having some trouble getting zinc plating going… I...
  2. Plating Titanium with Black Krome First, let me say that I am considering purchasing the...
  3. Problems with anodizing 356 castings! Hey folks. I’ve been doing lots of searches on here...
  4. Aluminum Coatings Can you sell this or do you offer something similar??...
  5. Noobie here with some question. Hello everyone, I am new to the PC process. I...

Tags: , , , , , ,

Under metal finishing

Leave a Comment for ran into a problem??????

Required

Required, hidden

Subscribe to the comments via RSS Feed


Recent Blog Posts

Categories

Tags

Posts by Month

Blogroll