I have been plating with the original CopyCad solution for around 6 years now with fairly good results. My question is, does the solution wear out? I filter my solution after each plating session and I have eliminated all sources of rust contamination from fixtures, connectors etc. I have never been able to get bright parts, even when the bath was new. I have generally been plating at 25 ma per square inch and I plate typically for 1 hour. Yellow chormate works great but the black chromate does not. Also, I cannot get bright parts using the brightner. It simply doesn’t work.
So, again, could my bath be worn out?
Jerry Hudgens
Related posts:
- How do any of you get a Bright Shiny Finish with CopyCad? How do you get a bright, shiny finish with CopyCad?...
- Removing CopyCad How do you guys remove zinc/CopyCad from parts? I am...
- yellow cad look solution age?? Well my yellow liquid cad solution has been in the...
- Different Color Hues in Black Chromate? I recently bought a new CopyCad bath and have been...
- rose gold plating solution hi anyone, im wish to give clients the option of...
Tags: anodizing, coating, finishing, metal finishing, Plating, powder coating